Lost Wax Casting for Custom Rings: Step by Step
Bench notes · The Journal

A boutique in Vancouver wanted a 14K matte wedding band with a hidden hand-engraved message inside, produced from a single customer's wax carving. They asked whether we could just cast the carving directly. We could not explain why in one email, so we walked them through the investment-casting line: from tree to burnout to pour. This is the step-by-step that came out of that call, and it is the same sequence we run for every custom ring that leaves our bench.
01Step one: from CAD or wax to a sprue pattern
Modern custom rings almost never start with a hand-carved wax anymore. We mill or print a resin positive in the exact ring geometry, then attach it to a rubber base with wax sprues. The sprue is the channel metal will flow through, and its angle and diameter decide where porosity hides. For a 2 mm wide band we use a 1.5 mm sprue; for a solitaire head we angle the sprue toward the shank so the heavy head fills last. Getting this wrong is the number one cause of shrinkage voids under a solitaire seat.
02Step two: investment, burnout and the pour
The sprue tree goes into a steel flask and is poured over with a gypsum-bonded investment slurry. After it sets, the flask goes into a burnout oven for roughly 12 hours: a slow ramp to about 700 degrees Celsius that vaporizes the resin and leaves a hollow cavity. We then pour the metal, 14K, 18K, or platinum, into the still-hot flask under centrifugal or vacuum pressure. The hot flask stops the metal from freezing before it reaches the thinnest details, which is why a cold pour fails on filigree.
The alloy itself matters. For color choices across yellow, rose and white families, we reference our notes on gold alloy colors in custom jewelry, because the burnout curve shifts slightly between a high-copper rose and a high-silver white. After the flask cools, we break it out, cut the sprues off, and tumble the raw casting for 40 minutes before it hits the bench.
03Step three: bench, seat, and the first QC gate
A raw casting is not a ring yet. The bench jeweler files the sprue nub, rounds the shank, and aligns the two halves that meet at the parting line. Then comes the seat: cutting a precise bed for the center stone with a bud burr, usually to within 0.05 mm of the stone's girdle. We follow the stone geometry guidance published by the GIA 4Cs when we seat a customer-supplied diamond, because the table-to-girdle ratio changes how deep the seat must be. This stage is also where we check for casting porosity under 10x magnification; a void near a prong tip gets soldered shut before the stone goes in.
04Step four: setting, finishing and final polish
With the stone set and prongs burnished, the ring moves through rough sanding (220 grit) to fine finishing (600 grit) to a high polish on a muslin wheel. The last station is the ultrasonic and steam clean, then a final inspection under the loupe. We tie this stage to our own bench standards, which we detail in bench finishing and polishing standards, so boutiques know exactly what surface they are buying. For rings that must later be sized, see our notes on what ring resizing can and cannot do; the casting wall you leave now decides how much future sizing room you have.
How long does lost wax casting take for a single custom ring?
From approved CAD to a finished, set ring is typically 7 to 12 working days. The burnout and cooling alone take about 18 hours, and the bench work for a solitaire runs two to three days.
Can you cast directly from a customer's old ring?
We do not melt a customer's sentimental ring and cast from it directly. Instead we scan it, mill a new resin positive, and cast fresh alloy. This avoids hidden solder joints and contamination that can spoil a melt.
Why is my casting slightly lighter than the CAD weight?
Some shrinkage in the flask is normal, usually 3 to 7 percent for gold. We build that tolerance into the quote weight and will flag anything beyond 10 percent as a modeling error.
Does lost wax work for platinum as well as gold?
Yes, but platinum needs a higher burnout and a different investment. It runs roughly 30 percent longer in the oven and is priced separately. We cover alloy choices in 14K, 18K and silver trade-offs.
We run a full lost-wax line for boutiques, from resin print to set and polished ring, with a resin-approval step before every pour. If you want a casting partner that sends weight tickets and porosity logs with every order, ask about our private-label custom manufacturing program.
05Frequently Asked Questions
What ring sizes can you supply in bulk?
US sizes 5–12 including half sizes. Send a size breakdown with your order and we cast to that curve; comfort-fit inner bands reduce resize requests.
Can I order a mixed size run instead of one size?
Yes. Mixed runs are standard for wholesale: specify quantity per size and we pack and label by size at no extra labor cost.
What is the MOQ for custom ring designs?
50 pieces per design for existing molds; 100–300 pieces when a new mold or CAD model is required.
How should I price rings for retail margin?
Most partners use a 3–4x markup on FOB cost for sterling and 2.5–3x for moissanite solos, which keeps landed cost under 30% of retail.
Send a sketch or a photo — our setter will answer with stone options and a price band.
Talk to the atelier